Isocer® Ceramic Head - High wear resistance
2.4 mg / mio. load cycles with 36 mm Isocer® head against Vitelene® [1]
In vivo oxidation stability
Vitelene® with stable oxidation index up to 5 weeks of aging 70°C / O2 / 5 bar (ASTM F2003-02) [2]
Proven fracture resistance
Statistic / dynamic fracture resistance 89.3 kN / 72.6 kN IsocerR head 28L / TiAl6V4 12/14 [3]
More corrosion resistant taper connection
Reduced ion transfer of ceramic heads compared to metal heads [4]