Premium Dispersed Phase Amalgam Alloy: Fast & Regular Set
Long lasting, condensable alloy with high compressive strength
Ensures good marginal integrity
Eliminates open contacts
Provides longer lasting and corrosion resistant restorations
Requires no pinching or twisting of the capsule to open
Condensable alloy
Virtual elimination of gamma II
Self-activating capsule
Premium Dispersed Phase Amalgam Alloy Fast Set Physical Properties
Property - - Value
Metal Composition: - - - 53% Silver, 23% Tin, 24% Copper
Formulation: - - - Admix
Alloy Mercury Ratio: - - - 50% Alloy, 50% Mercury
Compressive Strength: - - - 1 Hour Strength: 23,000 psi, 24 Hour Strength: 58,000 psi
Static Creep: - - - 0.3%
Dimensional Change: - - - ± 0.5 microns/cm
Premium Dispersed Phase Amalgam Alloy Regular Set Physical Properties
Property - - Value
Metal Composition: - - - 53% Silver, 23% Tin, 24% Copper
Formulation: - - - Admix
Alloy Mercury Ratio: - - - 50% Alloy, 50% Mercury
Compressive Strength: - - - 1 Hour Strength: 23,000 psi, 24 Hour Strength: 58,000 psi
Static Creep: - - - 0.3%
Dimensional Change: - - - ± 0.5 microns/cm
Zenith Premium Dispersed Phase Amalgam Alloy is a long lasting, condensable alloy that exhibits excellent handling characteristics and high compressive strength.
The condensable alloy ensures good marginal integrity and eliminates open contacts while providing longer lasting and corrosion resistant restorations.